Welding and Weldment Metallurgy: Processes, Procedures, Inspection and Failure Prevention

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


 Course Overview

This 5-day corrosion short course aims to provide the participants with an understanding of welding, weldment metallurgy, the effects of various variables on weld quality and the requirements for pre-heating and postweld heat treatment. Also covered in this course are welding defects and weld inspection, weldment corrosion and failure analysis. 

 

This corrosion short course is available for in-house training, online and distance learning worldwide. It can also be customized to meet the specific needs of your organization.

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


 Course Outline
 

1. Introduction to Welding and Metallurgy
2. Welding Processes

    2.1 SMAW
    2.2 FCAW
    2.3 SAW
    2.4 GMAW
    2.5 ESW/EGW
3. Process Selection
    3.1 Joint Requirements
    3.2 Process Capabilities
    3.3 Special Situations
4. Welding Procedures
    4.1 Effects of Welding Variables
    4.2 Purpose of Welding Procedure Specifications
    4.3 Prequalified Welding Procedure Specifications
    4.4 Guidelines For Preparing Prequalified WPSs
    4.5 Qualifying Welding Procedures By Test
    4.6 Approval of WPSs
    4.7 Examples
5. Welding Techniques and Variables
    5.1 SMAW
    5.2 FCAW-ss
    5.3 FCAW-g
    5.4 SAW
    5.5 GMAW
    5.6 ESW/EGW
6. Welder Qualification
7. Welding Defects and Weld Inspection
    7.1 Welding Defetcs: Causes and Prevention
    7.2 Weld Inspection
8. Preheating & PWHT Requirements
    8.1 Equivalent Carbon Content (ECC)
    8.2 Preheating & PWHT Requirements for Carbon Steels
    8.3 Preheating & PWHT Requirements for Stainless Steels and Other Alloys
9. Weldment Metallurgy and Weldment Corrosion
    9.1 Factors Affecting Weldment Corrosion
    9.2 Methods of Welding
    9.3 Weld Defects
    9.4 Iron Contamination
    9.5 Heat Tint and Its Effect
    9.6 Weldment Corrosion of Various Alloys
    9.7 Weld Decay and Knifeline Attack
    9.8 Hydrogen Underbead Cracking
    9.9 Exfoliation
10. Failure Analysis & Prevention
11. End of Course Examination

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


Who Should Attend

This 5-day course provides an excellent avenue for designers, technical managers, inspection and maintenance engineers, coatings and weld inspectors, quality control personnel and anyone who is interested in welding, welding metallurgy, weldment corrosion, and failure analysis and its prevention.

 

Successful completion of this corrosion course helps participants prepare for their NACE certification examinations at the Corrosion Technician, Corrosion Technologist and Senior Corrosion Technologist levels.

 

 Registration for This  Corrosion Course
  • Click here to register for this corrosion course online, or

  • Click here to download this corrosion course brochure with registration form in PDF format.

 In-House Training Corrosion Courses

 

If you are concerned with corrosion in your business, in-house training is a great solution to train a group of employees from design, production, operation, quality assurance, inspection and maintenance, and technical sales and support on corrosion control and corrosion prevention technology. The contents of all corrosion courses can be customized to fit your organization's needs.

 

There is no minimum or maximum number of participants required for in-house training corrosion courses. We conduct the in-house training corrosion course at your company's premises and at a time convenient to your company. Requests for in-house training corrosion courses from overseas countries are also welcome.

 

Click here to contact us for a quotation.
 

 Corrosion Course-On-Demand

 

All our publicly scheduled corrosion short courses are conducted once a year. However, you do not need to wait for one year if you have missed any of the publicly scheduled corrosion courses as we have this unique corrosion course-on-demand scheme: we will conduct the course just for you on an one-on-one basis at a time and in a location convenient to you. This option costs significantly less than a full-scale in-house training program.

 

Click here to contact us for a quotation for taking this course as course-on-demand.

 

 Online and Distance Learning Corrosion Courses


All corrosion courses can be conducted through online or distance learning. An username and password will be emailed to course participants for accessing the online course materials. Alternatively, a CD-ROM containing the same online course material or a master hard copy of corrosion course notes can be sent to your organization. Instructions, course assignments, discussions and questions related to the corrosion courses are posted on the website. Free email support for online courses is provided for a period up to 12 months. A Certificate of Completion will be issued to participants who pass the online test with a score of 70% and above.

 

Click here to register this corrosion short course for online or distance learning.

 
 PowerPoint Slides and Test Banks for Trainers, Instructors, Tutors, University Lecturers and Professors

 

If you are involved in teaching corrosion courses, you may wish to purchase a complete set of PowerPoint slides and the computerized test banks (in MicroTest format) with solutions. These presentations are suitable for teaching corrosion courses at different levels (from undergraduate to postgraduate) and durations (from 6 hrs to 40 hrs). These ready-to-use corrosion PowerPoint slides contain high quality color photographs, illustrations, animations and video clips. They can also be easily edited and customized to your own styles. The corrosion test banks contain over 1,000 corrosion questions for your use in tutorials, tests or examinations. These questions are conveniently grouped into 4 categories in the test bank: (1) true or false, (2) multiple choice, (3) calculation, and (4) reasoning and open-ended discussions).

 

Click here to contact us if you need more information.

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


Home | Contact Us

Copyright 1995-2019. All rights reserved.