Corrosion Control and Prevention in
Seawater Desalination Plants

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


 Course Overview

 

Seawater is known to be the most corrosive environment in nature. Many engineering materials used in seawater desalination plants worldwide including stainless steels and alloys are susceptible to  various forms of corrosion such as crevice corrosion, pitting corrosion and stress corrosion cracking. This one-day corrosion short course aims to provide the participants with a thorough understanding of the causes of corrosion in seawater desalination systems and the state-of-the-art technology for corrosion control and prevention. Upon completion of this short course the participants will be able to identify different forms of corrosion, analyze the root causes of corrosion failures, apply appropriate methods and strategies for corrosion control and prevention in seawater desalination operations.

 

This corrosion short course is available for in-house training, online and distance learning worldwide. It can also be customized to meet the specific needs of your organization.

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


 Course Outline
 

1. Introduction to Seawater Desalination
   

    1.1 History of Seawater Desalination

    1.2 Overview of Seawater Desalination Processes
    1.3 Thermal Method of Desalination

           1.3.1 Multi-Stage Flash Distillation (MSF)

           1.3.2 Multi-Effect Distillation (MED)

    1.4 Membrane Method of Desalination

           1.4.1 Seawater Reverse Osmosis (SWRO)

           1.4.2 Electro-dialysis (ED)/Electrodialysis Reversal (EDR)

 

2. Corrosion: Basic Concepts and Terminology
 

3. The Corrosivity of Seawater


4. Corrosion in Seawater Desalination Plants
     4.1   Overview of Corrosion in Desalination
              Plants Worldwide
     4.2   Vapor Space Corrosion
     4.3   Corrosion in Flash Chambers
     4.4   Corrosion in Heat Exchangers
     4.5   Corrosion in Distillate Systems
     4.6   Corrosion in Ejectors and Ejector Condensers
     4.7   Corrosion in Venting Systems

     4.8   Corrosion in Pumps and Valves

     4.9   Corrosion in Intake Systems

     4.10 Corrosion in High Pressure Piping

 

5. Case Studies of Corrosion Failures in Seawater Reverse Osmosis (SWRO) Plants

 

6. Corrosion Control and Prevention in Seawater Desalination Plants
    6.1 Material Selection

           6.1.1 Plain Carbon and Low Alloy Steels

           6.1.2 Stainless Steels and Alloys

           6.1.3 Copper and Copper Alloys

           6.1.4 Nickel and Nickel Alloys

           6.1.5 Composite Materials
    6.2 Design Against Corrosion
    6.3 Control of Operations


7
. Corrosion Monitoring in Seawater Desalination Plants

 

Course Outline |Who Should Attend |Registration |In-House |On-Demand |Online Courses |PPT Slides+Testbank |Course List


 Who Should Attend

 

Owners and operators of seawater desalination plants, corrosion practitioners, designers, engineers, technical managers, inspection and maintenance engineers, quality control personnel and those involved in failure analysis.

 

 Registration for This  Corrosion Course

 

  • Click here to register for this corrosion course online, or

  • Click here to download this corrosion course brochure with registration form in PDF format.

 In-House Training Corrosion Courses

 

If you are concerned with corrosion in your business, in-house training is a great solution to train a group of employees from design, production, operation, quality assurance, inspection and maintenance, and technical sales and support on corrosion control and corrosion prevention technology. The contents of all corrosion courses can be customized to fit your organization's needs.

 

There is no minimum or maximum number of participants required for in-house training corrosion courses. We conduct the in-house training corrosion course at your company's premises and at a time convenient to your company. Requests for in-house training corrosion courses from overseas countries are also welcome.

 

Click here to contact us for a quotation.

 

 Corrosion Course-On-Demand

 

All our publicly scheduled corrosion short courses are conducted once a year. However, you do not need to wait for one year if you have missed any of the publicly scheduled corrosion courses as we have this unique corrosion course-on-demand scheme: we will conduct the course just for you on an one-on-one basis at a time and in a location convenient to you. This option costs significantly less than a full-scale in-house training program.

 

Click here to contact us for a quotation for taking this course as course-on-demand.

 

 Online and Distance Learning Corrosion Courses


All corrosion courses can be conducted through online or distance learning. An username and password will be emailed to course participants for accessing the online course materials. Alternatively, a CD-ROM containing the same online course material or a master hard copy of corrosion course notes can be sent to your organization. Instructions, course assignments, discussions and questions related to the corrosion courses are posted on the website. Free email support for online courses is provided for a period up to 12 months. A Certificate of Completion will be issued to participants who pass the online test with a score of 70% and above.

Click here to register this corrosion short course for online or distance learning.

 
 PowerPoint Slides and Test Banks for Trainers, Instructors, Tutors, University Lecturers and Professors

 

If you are involved in teaching corrosion courses, you may wish to purchase a complete set of PowerPoint slides and the computerized test banks (in MicroTest format) with solutions. These presentations are suitable for teaching corrosion courses at different levels (from undergraduate to postgraduate) and durations (from 6 hrs to 40 hrs). These ready-to-use corrosion PowerPoint slides contain high quality color photographs, illustrations, animations and video clips. They can also be easily edited and customized to your own styles. The corrosion test banks contain over 1,000 corrosion questions for your use in tutorials, tests or examinations. These questions are conveniently grouped into 4 categories in the test bank: (1) true or false, (2) multiple choice, (3) calculation, and (4) reasoning and open-ended discussions).

 

Click here to contact us if you need more information.

 